Welcome to Zhengzhou Xinli Wear-Resistant Material Co. Ltd.
The tabular alumina powder takes the imported industrial alumina powder as the main material. Through special processing, grain growth direction is controlled by high temperature, the particles appears the unique plate-like structure, mohs hardness is up to 9 degree, it has the strong grinding force, not easy to produce scratches.
The tabular alumina powder takes the imported industrial alumina powder as the main material. Through special processing, grain growth direction is controlled by high temperature, the particles appears the unique plate-like structure, mohs hardness is up to 9 degree, it has the strong grinding force, not easy to produce scratches.
Polishing powder for high-precision electronic materials, grinding and polishing for monocrystalline silicon wafers, piezoelectric quartz crystals, and compound semiconductors.
As the filler to increase thermal conductivity of polymer.
As the reinforcer for improving fracture toughness of ceramics.
Pearlescent pigment substrate that is better than mica.
Additives for cosmetics.
Grains(μm) | Grain distribution | Packing(kg) | |||
D0 | D3 | D50 | D94 | ||
45 | <82.9 | 53.4±3.2 | 34.9±2.3 | 22.8±1.8 | 20 |
40 | <77.8 | 41.8±2.8 | 29.7±2.0 | 19.0±1.0 | 20 |
35 | <64.0 | 37.6±2.2 | 25.5±1.7 | 16.0±1.0 | 20 |
30 | <50.8 | 30.2±2.1 | 20.8±1.5 | 14.5±1.1 | 20 |
25 | <40.3 | 26.3±1.9 | 17.4±1.3 | 10.4±0.8 | 20 |
20 | <32.0 | 22.5±1.6 | 14.2±1.1 | 9.00±0.80 | 20 |
15 | <25.4 | 16.0±1.2 | 10.2±0.8 | 6.30±0.50 | 20 |
12 | <20.2 | 12.8±1.0 | 8.20±0.60 | 4.90±0.50 | 20 |
9 | <16.0 | 9.70±0.80 | 6.40±0.50 | 3.60±0.30 | 20 |
5 | <12.7 | 7.20±0.60 | 4.70±0.40 | 2.80±0.25 | 20 |
3 | <10.1 | 5.20±0.40 | 3.10±0.30 | 1.80±0.30 | 20 |
2 | <8.5 | 4.20±0.30 | 2.50±0.30 | 0.90±0.20 | 20 |
1 | <5.5 | 3.50±0.30 | 1.50±0.30 | 0.30±0.30 | 20 |